摘要 |
<p>alloys, suitable as deoxidation alloy for steel, or for prodn. of Si, SiCa and Fe-poor iron alloys, are obtained by using a charge comprising a mixture of petroleum coke and anthracite at a ratio of anthracite to petroleum coke of 2.85 to 0.7-1. referred to the non-volatile carbon. The charge pref. contains in addition a binding agent composed of sulphite-alcohol extract based on Na, Mg or ammonium cations and may also contain chlorides and fluorides of alkali-or alkaline earth metals in amounts of 3% of total wt. of charge.</p> |
申请人 |
WSESOJUSNIJ NAUTSCHNO-ISSLEDOWATEL'SKIJ I PROJEKTNIJ INSTITUT ALJUMINIEWOJ,MAGNIEWOJ I ELEKTRODNOJ PROMYSCHLENNOSTI |
发明人 |
I. BRUSAKOW,JURIJ;P. KISELEW,WASILIJ;A. RSCHAWIN,SERGEJ;M. WARJUSCHENKOW,ANATOLIJ;W. IL'INKOW,DMITRIJ;I. WOL'PIN,PAWEL;I. RAGULINA GEB. GORBUNOWA,RAISA;P. AWDEEW,MICHAIL;A. ARTEMENKO,STANISLAW;P. ISAEWA GEB. MEL'ZER,ELENA;S. TARASOW,MICHAIL;M. RAPOPORT,WLADIMIR;A. BERESCHNOJ,IWAN;P. RUMJANZEW,WASILIJ;S. SCHPAK,GRIGORIJ;S. GUS,DMITRIJ;W. TIMOFEEW,WLADIMIR;CH. ALIWOJWODITSCH,MIRO;P. CHRENNIKOWA GEB. ISAEWA,LJUDMILA;G. KUTSCHERENKO,ANATOLIJ |