发明名称 |
Smokable material and method for preparing same |
摘要 |
A smokable material formed by heating a cellulosic or carbohydrate material at a temperature within the range of 150 DEG -750 DEG C in an inert, non-oxidizing atmosphere for a time sufficient to effect a weight loss of at least 60% but not more than 90%.
|
申请公布号 |
US4019521(A) |
申请公布日期 |
1977.04.26 |
申请号 |
US19750562735 |
申请日期 |
1975.03.27 |
申请人 |
PHILIP MORRIS INCORPORATED |
发明人 |
BRISKIN, THEODORE S. |
分类号 |
A24B15/16;(IPC1-7):A24B15/00 |
主分类号 |
A24B15/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|