发明名称 METHOD OF OBTAINING A CRYSTALLINE LAMELLAR STRUCTURE
摘要 PCT No. PCT/PL94/00008 Sec. 371 Date Feb. 9, 1996 Sec. 102(e) Date Feb. 9, 1996 PCT Filed Apr. 27, 1994 PCT Pub. No. WO95/04845 PCT Pub. Date Feb. 16, 1995A process for fabricating a multilayer crystalline structure of nitrides of metals from group III of periodic table including GaN, AlN and InN is provided. The process includes the steps of heating a group III metal (26) to a temperature T1 under an equilibrium nitrogen pressure while maintaining group III metal nitride stability to form a first crystal layer of the group III metal nitride. Thereafter the method includes the step of forming a second crystal layer (28) of the group III metal nitride by decreasing the nitrogen pressure such that the second crystal layer grows on the first layer with a growth rate slower than the growth rate of the first layer at a temperature T2 not greater than temperature T1. The second layer (28) grows on at least a portion of the first layer at a predetermined thickness under the new nitrogen pressure.
申请公布号 PL173917(B1) 申请公布日期 1998.05.29
申请号 PL19930300019 申请日期 1993.08.10
申请人 CENTRUM BADAN WYSOKOCISNIENIOWYCH PAN 发明人 POROWSKI SYLWESTER;JUN JAN;GRZEGORY IZABELLA;KRUKOWSKI STANISLAW;WROBLEWSKI MIROSLAW
分类号 C30B29/40;C23C16/18;C30B11/00;C30B11/12;H01L21/20;H01L21/203;H01L21/205;H01L21/208;H01L33/00;H01L33/32;H01S5/00;H01S5/323 主分类号 C30B29/40
代理机构 代理人
主权项
地址