摘要 |
The invention relates to a method for coating textiles and/or leather with an aqueous dispersion comprising (A) a mixture of (i) a urethane-containing blocked NCO prepolymer having a number average molecular weight of 2000 to 10,000, a content of blocked isocyanate groups (calculated as NCO) of 0.5 to 5 wt.%, an ethoxy group content of 2 to 50 wt.%, an ionic group content of 5 to 30 meq per 100 g of the prepolymer, and (ii) a polyamine having (cyclo)aliphatically bonded primary and/or secondary amino groups, wherein the equivalent ratio of blocked NCO groups of component (i) to amino groups of component (ii) is 1:0.9 to 1:1.2, and (B) an aqueous phase.
|