发明名称 СПОСОБ ИЗВЛЕЧЕНИЯ МЕДИ ИЗ РУДЫ МЕСТОРОЖДЕНИЯ УДОКАН
摘要 FIELD: metallurgy. ^ SUBSTANCE: method involves processing with solution containing sulphuric acid, and flushing with water. Ore or concentrate are reduced to 0.1-0.7 mm grade before processing. Processing is performed in 2-4-stage counterflow by leach solution containing sulphuric acid and copper sulphate at molar ratio of oxidised copper in ore or concentrate: sulphuric acid = 1:1.3-2.0, at solid : liquid ratio within 1:1-4 at each stage. Processed ore is flushed in counterflow by water in 2-4 at ore or ore concentrate to water ratio = 2-5:1 and solid : liquid ratio within 1:1-4 at each stage. Sulphuric acid is added to the water solution obtained after flushing and containing sulphuric acid and copper sulphate till sulphuric acid concentration reaches 10-40 g/dm3, and source ore or ore concentrate is processed with obtained solution. ^ EFFECT: increased copper concentration in product solution. ^ 2 tbl, 2 ex
申请公布号 RU2007107213(A) 申请公布日期 2008.09.10
申请号 RU20070107213 申请日期 2007.02.27
申请人 Вальков Александр Васильевич (RU) 发明人 Вальков Александр Васильевич (RU)
分类号 C22B3/04 主分类号 C22B3/04
代理机构 代理人
主权项
地址