PROBLEM TO BE SOLVED: To provide an ASA resin composition good in molding appearance and excellent in excoriation resistance and creak reduction effect without needs for hard cording after molding.SOLUTION: There is an ASA resin composition containing (A) an ASA resin and (B) a graft copolymer of 0.5 to 20 pts.wt. based on the (A) component, where the (B) graft copolymer has polyethylene as a main chain and polystyrene as a side chain and a component of the graft copolymer consisting of a polyethylene component of 40 to 90 wt.% and a polystyrene component of 10 to 60 wt.%.SELECTED DRAWING: None |