发明名称 ELECTROPOLISHING PROCESS FOR TITANIUM
摘要 PROBLEM TO BE SOLVED: To provide a method of electropolishing, with which titanium and titanium-containing alloys such as Nitinol can be smoothed and deburred efficiently and at high quality, without causing any appreciable pollution or dangers for humans and the environment, and making expensive cooling equipment and safety precautions unnecessary. SOLUTION: An electrolyte including methanesulfonic acid and one or more alkanediphosphonic acids is used. The electropolishing preferably takes place at a temperature in the range from 20°C to 70°C, for example between room temperature and 60°C, and in particular at a temperature between 25°C and 50°C. The anodic current density at which the workpieces are electropolished is preferably in the range from 2 to 50 A/dm<SP>2</SP>, in particular between 5 to 30 A/dm<SP>2</SP>. The applied voltage can often be in the range from 10 to 35 V. COPYRIGHT: (C)2008,JPO&INPIT
申请公布号 JP2008223139(A) 申请公布日期 2008.09.25
申请号 JP20080057258 申请日期 2008.03.07
申请人 POLIGRAT GMBH 发明人 BOHME OLAF;PIESSLINGER-SCHWEIGER SIEGFRIED
分类号 C25F3/26;B23H5/08 主分类号 C25F3/26
代理机构 代理人
主权项
地址