发明名称 High belite-containing sulphoaluminous clinker, method for the production and the use thereof for preparing hydraulic binders
摘要 <p>A sulphoaluminate clinker includes as a phasic formulation, compared with the total weight of clinker: 5 to 25% of a calcium aluminoferrite phase with a formulation corresponding to the general formula C2AXF(1−X), with X comprised between 0.2 and 0.8; 15 to 35% of a calcium sulphoaluminate phase yee' limit (C4A3$); 40 to 75% belite (C2S); from 0.01 to 10% of one or several minor phases selected from the group consisting of calcium sulphates, alkali sulphates, perovskite, calcium aluminates, gehlenite, free lime and periclase, and/or a vitreous phase, and additives including at least sodium and boron present in the following quantities, by weight as compared to the total weight of the clinker: from 0.1 to 5% of sodium expressed as sodium oxide and from 0.2 to 3% of boron, expressed as boron oxide, the total content of said additives being less than or equal to 15%.</p>
申请公布号 KR101164901(B1) 申请公布日期 2012.07.23
申请号 KR20077003969 申请日期 2005.07.19
申请人 发明人
分类号 C04B7/32;C04B28/06 主分类号 C04B7/32
代理机构 代理人
主权项
地址