发明名称 |
TONER AND EXTERNAL ADDITIVE FOR TONER |
摘要 |
Provided is a toner, including: a toner particle; and an organic-inorganic composite fine particle on a surface of the toner particle, in which the organic-inorganic composite fine particle includes: a resin fine particle; and an inorganic fine particle embedded in the resin fine particle, and part of which is exposed to a surface of the composite fine particle, and in which the composite fine particle satisfies the following relationships: (i) in viscoelasticity measurement of the composite fine particle, when the loss elastic modulus thereof at a temperature T (° C.) is represented by G″T [dN/m2], a change ratio d(Log(G″T))/dT of a common logarithm of the loss elastic modulus has a minimum in a temperature range of from 60° C. to 150° C., and the minimum is less than −0.10; and (ii) the loss elastic modulus (G″180) thereof at a temperature of 180° C. is 1.0×104 dN/m2 or more and 1.0×107 dN/m2 or less. |
申请公布号 |
US2016202624(A1) |
申请公布日期 |
2016.07.14 |
申请号 |
US201514975495 |
申请日期 |
2015.12.18 |
申请人 |
CANON KABUSHIKI KAISHA |
发明人 |
Nishikawa Koji;Moribe Shuhei;Yoshiba Daisuke;Nomura Shotaro;Fukudome Kosuke;Akiyama Hiroki;Hotta Yojiro;Yamazaki Katsuhisa |
分类号 |
G03G9/097 |
主分类号 |
G03G9/097 |
代理机构 |
|
代理人 |
|
主权项 |
1. A toner, comprising:
a toner particle; and an organic-inorganic composite fine particle on a surface of the toner particle, wherein the organic-inorganic composite fine particle comprises:
a resin fine particle; andan inorganic fine particle which is embedded in the resin fine particle, and part of which is exposed to a surface of the organic-inorganic composite fine particle, and wherein the organic-inorganic composite fine particle satisfies the following relationships (i) and (ii): (i) in viscoelasticity measurement of the organic-inorganic composite fine particle, when a loss elastic modulus thereof at a temperature T (° C.) is represented by G″T [dN/m2] and a change ratio of a common logarithm of the loss elastic modulus is represented by d(Log(G″T))/dT, the d(Log(G″T))/dT has a minimum in a temperature range of from 60° C. 150° C., and the minimum is less than −0.10; and (ii) in the viscoelasticity measurement of the organic-inorganic composite fine particle, when a loss elastic modulus thereof at a temperature of 180° C. is represented by G″180, the G″180 is 1.0×104 dN/m2 or more and 1.0×107 dN/m2 or less. |
地址 |