发明名称 |
AUSTENITIC IRON/NICKEL/CHROMIUM/COPPER ALLOY |
摘要 |
The invention relates to an austenitic iron/nickel/chromium/copper alloy, the composition of which comprises in % by weight: 24% = Ni = 36%; Cr = 0.02%; Cu = 0.1%; Cu + Co = 15%; 0.01 = Mn = 6%; 0.02 = Si = 2%; 0 = Al + Ti = 3%; 0 = C = 2%; 0 = V + W = 6%; 0 = Nb + Zr = 0.5%; 0 = Mo = 8; Sn = 1; 0 = B = 0.006%; 0 = S + Se + Sb = 0.008%; 0 = Ca + Mg = 0.020%; the reminder being iron and impurities resulting from the smelting, the percentages of nickel, chromium, copper and cobalt being such that the alloy also meets the following conditions: Co < Cu; Co < 4% if Cr > 7.5%; Eq1 > 28% where Eq1 = Ni + 1.2 Cr + (Cu/5); Cr < 7.5% if Ni > 32.5%, and the manganese content also meeting the following conditions : if Eq3 = 205, Mn = Ni - 27.5 + Cu - Cr; if 180.5 = Eq3 = 205, Mn = 4%; if Eq3 = 180.5, Mn < 2% where Eq3 = 6Ni - 2.5X + 4(Cu+Co) and X = Cr+Mo+V+W+Si+Al. |
申请公布号 |
WO2008142229(A3) |
申请公布日期 |
2009.03.19 |
申请号 |
WO2008FR00403 |
申请日期 |
2008.03.26 |
申请人 |
ARCELORMITTAL-STAINLESS AND NICKEL ALLOYS;WAECKERLE, THIERRY;DANYLOVA, OLENA |
发明人 |
WAECKERLE, THIERRY;DANYLOVA, OLENA |
分类号 |
C22C38/08;C22C19/00;H01F10/12 |
主分类号 |
C22C38/08 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|