发明名称 |
METHOD OF MANUFACTURING LIQUID-COOLED JACKET |
摘要 |
A method of manufacturing a liquid-cooled jacket, includes a preparation step which includes placing a sealing body on a stepped portion to allow a step side surface and a sealing-body side surface of the sealing body to butt each other, and a primary joining step which includes allowing a primary joining rotary tool to move once around the sealing body, while moving the rotary tool along a butted portion formed in the preparation step, to carry out friction stir welding. The primary joining step includes employing the primary joining rotary tool provided with a stirring pin having a length dimension greater than a thickness dimension of the sealing body, and carrying out friction stirring with only the stirring pin being brought into contact with a jacket body and the sealing body. |
申请公布号 |
US2016325374(A1) |
申请公布日期 |
2016.11.10 |
申请号 |
US201415111191 |
申请日期 |
2014.08.27 |
申请人 |
NIPPON LIGHT METAL COMPANY, LTD. |
发明人 |
HORI Hisashi;SEO Nobushiro |
分类号 |
B23K20/12 |
主分类号 |
B23K20/12 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method of manufacturing a liquid-cooled jacket which is composed of a jacket body having a bottom portion and a frame-shaped side wall portion provided to stand on the bottom portion, and a sealing body which seals an opening of the jacket body, and allows heat transport fluid to flow in a hollow portion formed by the jacket body and the sealing body, the method comprising:
a preparation step which includes forming, on a peripheral edge of the opening of the jacket body, a step bottom surface located below by one step from an end surface of the side wall portion, and a step side surface rising from the step bottom surface, and placing the sealing body on the step bottom surface to allow the step side surface and a sealing-body side surface of the sealing body to butt each other; and a primary joining step which includes allowing a rotary tool to move once around the sealing body, while moving the rotary tool along a butted portion formed in the preparation step, to carry out friction stir welding, wherein the primary joining step includes employing the rotary tool provided with a stirring pin having a length dimension greater than a thickness dimension of the sealing body, and carrying out friction stirring with only the stirring pin being brought into contact with the jacket body and the sealing body. |
地址 |
Tokyo JP |