摘要 |
A solid explosive composition is made by curing a mixture of a from about 20% to about 50% by weight of a liquid matrix, from about 50% to about 80% by weight of a dry or monohydrate inorganic chlorate or perchlorate salt, and from 0% to about 22% of a salt selected from the group consisting of nitrate oxidizer salts and inert chloride salts, after transferring said mixture to a mold. The matrix can include from about 50% to about 84% by weight of a non-explosive liquid fuel selected from the group consisting of polyhydric alcohols, lower aliphatic alcohols, ketones, and hydrocarbons; from 0% to about 15% by weight of a nitrate oxidizer salt; from 0% to about 15% by weight water; from 0% to about 15% by weight of a thickener; from 0% to about 5% by weight of an acid; and from 0% to about 2% by weight of a surfactant. |