发明名称 Corrosion resistant alloy
摘要 Alloys are provided which consist essentially of between about 4% and 18.5% by weight nickel, from about 24% to about 30% by weight chromium, from about 0.35 to about 1% by weight molybdenum, from about 2.7% to about 4.5% by weight copper, from about 2.7% to about 4.5% by weight silicon, up to about 1.5% by weight manganese, up to about 0.25% by weight nitrogen, up to about 0.8% by weight columbium (niobium), up to about 1.0% by weight tantalum, up to about 0.007% by weight boron, up to about 0.35% by weight vanadium, up to about 0.8% by weight tungsten, up to about 0.08% by weight carbon, up to about 0.6% by weight titanium and the balance essentially iron. Small amounts of cobalt as naturally occur in some ores may be present but are considered a part of the nickel content.
申请公布号 US4917860(A) 申请公布日期 1990.04.17
申请号 US19890295275 申请日期 1989.01.10
申请人 CARONDELET FOUNDRY COMPANY 发明人 CULLING, JOHN H.
分类号 C22C38/42 主分类号 C22C38/42