摘要 The method comprises providing a side glass felt layer (3) incorporating a thermo hardening resin, where the side layer shows a relative stress-strain characteristic in compression to be lower than 0.3 kPa, providing a back polyurethane foam layer (4) with a density of 8-15 g/l and a relative stress-strain characteristic in compression to be 3-25 kPa, hot compressing the felt layer and the polyurethane foam layer stacked one upon the other in a mold. The backing layer has an air resistance of lower than 5000 N.s.m 3>. The method comprises providing a side glass felt layer (3) incorporating a thermo hardening resin, where the side layer has a relative stress-strain characteristic in compression to be lower than 0.3 kPa, providing a back polyurethane foam layer (4) with a density of 8-15 g/l and a relative stress-strain characteristic in compression to be 3-25 kPa, hot compressing the felt layer and the polyurethane foam layer stacked one upon the other in a mold. The backing layer has an air resistance of lower than 5000 N.s.m 3>. The method further comprises: arranging a side coating layer (5) provided with a porous thermosetting adhesive on the felt layer before hot compression; and arranging a back coating layer (6) provided with a porous thermosetting adhesive on the foam layer before hot compression. An independent claim is included for an acoustic shield.
申请公布号 FR2980734(B1) 申请公布日期 2016.10.21
申请号 FR20110058876 申请日期 2011.09.30
申请人 CENTRE D'ETUDE ET DE RECHERCHE POUR L'AUTOMOBILE (CERA) 发明人 WAXIN LAURENT;LECOMTE ALICIA;LHERMITE YANN
分类号 B29C70/46;B32B27/12;B60R13/08;F02B77/13;G10K11/168 主分类号 B29C70/46
代理机构 代理人
主权项
地址