发明名称 |
BREAK-IN COATING ON TRACK ASSEMBLY COMPONENTS |
摘要 |
During the break-in period of track (22) assembly components, galling can occur between the components during use. The components include a pin (68) that is received within a bushing (70) and alternatively a sleeve bearing (74) between the pin (68) and the bushing (70) depending on the load. A method to prevent or reduce galling includes applying a coating (78) of zinc phosphate and a low-friction layer (76) on top of the zinc phosphate (78). The low-friction coating (76) can be made of WS2 (Tungsten Disulphide), BN (Boron Nitride), MoS2 (Molybdenum disulfide) or PTFE (Polytetrafluoroethylene) and deposited during a mechanical treatment. |
申请公布号 |
WO2016153622(A1) |
申请公布日期 |
2016.09.29 |
申请号 |
WO2016US17501 |
申请日期 |
2016.02.11 |
申请人 |
CATERPILLAR INC. |
发明人 |
FENG, Bao;DIEKEVERS, Mark S.;BAAR, William;WEAVER, Douglas;YOON, Hyung |
分类号 |
B62D55/21;C09D5/00;C10M169/04;C23C22/12;C23C22/83;C23C24/08;C23C28/00 |
主分类号 |
B62D55/21 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|