发明名称 Method for producing rubber composition
摘要 A method for producing a rubber composition that can improve wet grip performance is provided. The rubber composition includes 100 parts by mass of a rubber component, from 20 to 150 parts by mass of silica, and from 1 to 10 parts by mass of a polymer gel as crosslinked diene polymer particles, wherein from 30 to 90 parts by mass of at least one modified diene rubber selected from the group consisting of a styrene-butadiene rubber, a butadiene rubber and a natural rubber, each having introduced therein a functional group having an interaction with the silica, and from 70 to 10 parts by mass of an unmodified dine rubber are used as 100 parts by mass of the rubber component, and a polymer gel having a functional group which has an interaction with a functional group of the modified diene rubber is used as the polymer gel.
申请公布号 US9611381(B2) 申请公布日期 2017.04.04
申请号 US201514877371 申请日期 2015.10.07
申请人 TOYO TIRE & RUBBER CO., LTD. 发明人 Taniguchi Sho
分类号 C08L9/00;C08L9/06;C08L7/00;B60C1/00;C08J3/20;C08L15/00 主分类号 C08L9/00
代理机构 Westerman, Hattori, Daniels & Adrian, LLP 代理人 Westerman, Hattori, Daniels & Adrian, LLP
主权项 1. A method for producing a rubber composition, the rubber composition including 100 parts by mass of a rubber component, from 20 to 150 parts by mass of silica, and from 1 to 10 parts by mass of a polymer gel which is crosslinked diene polymer particles, wherein from 30 to 90 parts by mass of at least one modified diene rubber selected from the group consisting of a styrene-butadiene rubber, a butadiene rubber, and a natural rubber, each having introduced therein at least one functional group selected from the group consisting of a hydroxyl group, an amino group, a carboxyl group, an alkoxyl group, and an epoxy group, and from 70 to 10 parts by mass of an unmodified diene rubber are used as 100 parts by mass of the rubber component, a polymer gel having a glass transition temperature of from −40 to −10° C. and having at least one functional group selected from the group consisting of a hydroxyl group, an amino group, a carboxyl group, an alkoxyl group, and an epoxy group is used as the polymer gel, and the method comprises a first step of mixing the entire amount of the modified diene rubber with the polymer gel together with the silica to obtain a first mixture, and a second step of mixing the unmodified diene rubber with the first mixture obtained.
地址 Osaka-shi, Osaka JP
您可能感兴趣的专利