发明名称 MAGNETIC RECORDING MEDIUM AND MAGNETIC RECORDING AND REPRODUCING APPARATUS
摘要 In a magnetic recording medium of the present invention, an outermost surface of a protective layer 3 on a lubricant layer 4 side contains carbon and nitrogen in a range of 50 atomic % to 90 atomic %, and the lubricant layer 4 is formed by being in contact with the outermost surface, contains compounds A to C represented in the below general formulas (1) to (3) described below, and has a film thickness of 0.5 nm to 2 nm.;R1-C6H4OCH2CH(OH)CH2OCH2—R2-CH2OCH2CH(OH)CH2OH   (1),;CH2(OH)CH(OH)CH2OCH2CF2CF2(OCF2CF2CF2)mOCF2CF2CH2OCH2CH(OH)CH2OH   (2),;HOCH2CF2CF2O(CF2CF2CF2O)sCF2CF2CH2OCH2CH(OH)CH2OH   (3)
申请公布号 US2017084305(A1) 申请公布日期 2017.03.23
申请号 US201615264988 申请日期 2016.09.14
申请人 SHOWA DENKO K.K. 发明人 YAMAKAWA Eishin;TO Katsuaki;HAYASE Saeko
分类号 G11B19/28;G11B5/73;G11B21/10 主分类号 G11B19/28
代理机构 代理人
主权项 1. A magnetic recording medium comprising at least a magnetic layer, a protective layer, and a lubricant layer on a nonmagnetic substrate in this order, wherein an outermost surface of the protective layer on the lubricant layer side contains carbon and nitrogen, the nitrogen is contained in the outermost surface in a range of 50 atomic % to 90 atomic %, the lubricant layer is formed by being in contact with the outermost surface, has an average film thickness of 0.5 nm to 2 nm, and contains a compound A represented in the below general formula (1), a compound B represented in the below general formula (2), and a compound C represented in the below general formula (3), and a mass ratio (A/(A+B+C)) of the compound A with respect to a s of masses of the compounds A, B, and C contain d in the lubricant layer is in a range of 0.05 to 0.6, a mass ratio (B/(A+B+C)) of the compound B with respect to the sum of the masses of the compounds A, B, and C contained in the lubricant layer is in a range of 0.05 to 0.5, and a mass ratio (C/(A+B+C)) of the compound C with respect to the sum of the masses of the compounds A, B, and C contained in the lubricant layer is in a range of 0.05 to 0.9, R1-C6H4OCH2CH(OH)CH2OCH2—R2-CH2OCH2CH(OH)CH2OH   (1) in the general formula (1), R1 is an alkoxy group having 1 to 4 carbon atoms, R2 is —CF2O(CF2CF2O)x(CF2O)yCF2— (an order in parentheses of x and y may be this order, the opposite order, or a random order (each of x and y is an integer of 0 to 15).) CH2(OH)CH(OH)CH2OCH2CF2CF2(OCF2CF2CF2)mOCF2CF2CH2OCH2CH(OH)CH2OH   (2) in the general formula (2), m is an integer in a range of 4 to 50, HOCH2CF2CF2O(CF2CF2CF2O)sCF2CF2CH2OCH2CH(OH)CH2OH   (3) in the general formula (3), s is an integer.
地址 Tokyo JP