摘要 |
A process for producing a geopolymer includes combusting at least one of oil shale and mineral residues originating from a production of oil using the oil shale so as to produce a combustion product. The combustion product is ground. An alkaline activator is added to the combustion product to form a geopolymer mixture. Water is added to the geopolymer mixture. The geopolymer mixture is adjusted so as to obtain a mol ratio of Si:Al of 2 to 5, a mol ratio of K:Al of 0.6 to 0.7, a mol ratio of Si:K of 3 to 10, a mol ratio of Ca:Al of 0.1 to 0.4, and a mol ratio of Si:CA of 4.9 to 41. The geopolymer mixture is hardened. |