摘要 |
PROBLEM TO BE SOLVED: To provide a thin molded part having excellent heat resistance, impact resistance and bending resistance, and having a thin part in which the thinnest part has a thickness of 1 mm or lower.SOLUTION: There is provided a thin molded part having a thin part in which the thinnest part has a thickness of 1 mm or lower, in which a polycarbonate resin composition containing, to 100 pts.mass of a polycarbonate resin (A) containing a polycarbonate resin with a viscosity average molecular weight of 7,000 to 12,000 in 20 mass% or higher, a core/shell type elastomer (B) including acrylic core/acrylic shell in 3 to 15 pts.mass is molded. |