发明名称 |
Flooded lead-acid battery |
摘要 |
A flooded lead-acid battery, including a negative electrode plate holding a negative active material, a positive electrode plate holding a positive active material, and a flowable electrolyte solution in which these plates are immersed, and allowing the electrolyte solution to have a utilization factor greater than or equal to 75%, wherein the concentration of an alkali metal ion or an alkaline earth metal ion in the electrolyte solution is allowed to be 0.07 to 0.3 mol/L, and the pore volume of the negative active material after formation is allowed to be 0.08 to 0.16 mL/g. |
申请公布号 |
US9570779(B2) |
申请公布日期 |
2017.02.14 |
申请号 |
US201314767457 |
申请日期 |
2013.11.22 |
申请人 |
GS Yuasa International Ltd. |
发明人 |
Wada Hidetoshi;Hosokawa Masaaki |
分类号 |
H01M10/06;H01M4/14;H01M10/08;H01M2/16 |
主分类号 |
H01M10/06 |
代理机构 |
Rankin, Hill & Clark LLP |
代理人 |
Rankin, Hill & Clark LLP |
主权项 |
1. A flooded lead-acid battery, comprising a negative electrode plate holding a negative electrode material, a positive electrode plate holding a positive electrode material, and a flowable electrolyte solution in which these plates are immersed, and allowing the electrolyte solution to have a utilization factor greater than or equal to 75%, wherein
the concentration of an alkali metal ion or an alkaline earth metal ion in the electrolyte solution is 0.07 to 0.3 mol/L, and the pore volume of the negative electrode material is 0.08 to 0.16 mL/g. |
地址 |
Kyoto JP |