摘要 |
The process, according to the invention, comprises the following stages: (a) processing (1) of the laterite ore (O) by crushing, scrubbing, attrition, separation, and high-intensity magnetic separation; (b) Leaching (2) of the non-magnetic fraction (CN) obtained form the previous stage (a); (c) optionally, neutralization (3) of the effluent from the leaching and/or solid-liquid separation stages (4); (d) treatment of the effluents from stages (b) or (c) using an ion-exchange hybrid system (5) comprising at least one circuit for removal of impurities and at least one circuit for recovery of nickel and cobalt; (e) elution (6) of the ion-exchange resin used; (f) separation, purification, and recovery (7) of the nickel and cobalt. |