摘要 |
PROBLEM TO BE SOLVED: To provide a laminated film excellent in corrosion resistance to aminosilanes.SOLUTION: In the laminated film, a printing layer, an aluminum foil layer, a sealant layer and a coextrusion layer are bonded to the adjacent layers in this order. The printing layer is formed of a biaxially stretched polyethylene terephthalate or a biaxially oriented nylon, the aluminum foil layer has a thickness of 5 μm or more, the sealant layer is formed of a thermoplastic resin, and the coextrusion layer includes an ethylene/vinyl alcohol copolymer layer and a thermoplastic resin layer. |