发明名称 ECO-FRIENDLY INORGANIC COATING COMPOSITION AND PREPARATION METHODS THEREOF
摘要 Provided is an inorganic coating composition which comprises: 5-30 parts by weight of a hydrolyzable silane compound; 50-150 parts by weight of a water-dispersible polyurethane dispersing agent; 10-30 parts by weight of an acryl emulsion resin; and 5-120 parts by weight of a solvent, with respect to 100 parts by weight of a modified silane silicate composite. In addition, provided is a production method thereof. According to the present invention, the inorganic coating composition does not release harmful substances, and thus is eco-friendly. Furthermore, the composition forms a paint film which is physically and chemically stable on a surface of a target object needed to form the paint film, and enhances corrosion resistance as well.
申请公布号 KR20160012832(A) 申请公布日期 2016.02.03
申请号 KR20140095052 申请日期 2014.07.25
申请人 YANG, CHEOL HO 发明人 YANG, CHEOL HO;CHO, JAE SU
分类号 C09D1/00;C09D133/06;C09D183/02 主分类号 C09D1/00
代理机构 代理人
主权项
地址