发明名称 |
Polymer Compositions, Methods of Making the Same, and Articles Made Therefrom |
摘要 |
The present disclosure is directed to compositions and methods for improving the cling performance in stretch-cling films. Compositions include: (a) 80.0 to 99.5 wt. % of a propylene-based elastomer, the propylene-based elastomer comprising at least about 60.0 wt. % propylene-derived units and about 5.0 to about 25.0 wt. % ethylene-derived units, based on total weight of the propylene-based elastomer, wherein the propylene-based elastomer has a heat of fusion of less than about 80.0 J/g; and (b) 0.5 to 20.0 wt. % of a polyalphaolefin, wherein the amounts of the propylene-based elastomer, and the polyalphaolefin are based on the weight of the composition. Methods of making such compositions as well as compositions including an ethylene-based polymer and films and methods of making films are also disclosed. |
申请公布号 |
US2015030867(A1) |
申请公布日期 |
2015.01.29 |
申请号 |
US201414285050 |
申请日期 |
2014.05.22 |
申请人 |
ExxonMobil Chemical Patents Inc. |
发明人 |
German Paul M. |
分类号 |
C08J5/18;B32B27/32;B32B27/08 |
主分类号 |
C08J5/18 |
代理机构 |
|
代理人 |
|
主权项 |
1. A composition for improving the cling performance in stretch-cling films, the composition comprising:
(a) 80.0 to 99.5 wt. % of a propylene-based elastomer, the propylene-based elastomer comprising at least about 60.0 wt. % propylene-derived units and about 5.0 to about 25.0 wt. % ethylene-derived units, based on total weight of the propylene-based elastomer, wherein the propylene-based elastomer has a heat of fusion of less than about 80.0 J/g; and (b) 0.5 to 20.0 wt. % of a polyalphaolefin,wherein the amounts of the propylene-based elastomer and the polyalphaolefin are based on the weight of the composition. |
地址 |
Baytown TX US |