发明名称 HOLLOW FIBER MEMBRANE MODULE, METHOD FOR PRODUCING HOLLOW FIBER MEMBRANE, AND METHOD FOR PRODUCING HOLLOW FIBER MEMBRANE MODULE
摘要 An object of the present invention is to provide a dry-type hollow fiber membrane module which is excellent in blood compatibility and elutes little eluted substance, and a hollow fiber membrane built in the module, and a method for producing a hollow fiber membrane module. Disclosed is a hollow fiber membrane module including a built-in hollow fiber membrane including a hydrophobic polymer and a hydrophilic group-containing polymer, the hollow fiber membrane module satisfying the following items: (a) the water content of the hollow fiber membrane is 10% by weight or less relative to the tare weight of the hollow fiber membrane, (b) the hydrophobic polymer contains no nitrogen, the hydrophilic group-containing polymer contains nitrogen, and the nitrogen content of the hollow fiber membrane is 0.05% by weight or more and 0.4% byweight or less, (c) the content of the hydrophilic group-containing polymer in the inner surface of the membrane is 20% by weight or more and 45% by weight or less, and (d) the consumption amount of an aqueous potassium permanganate solution (2.0×10−3 mol/L) used for titrating an eluted substance in 10 mL of a last part of a priming liquid is 0.2 mL or less per 1 m2 of a membrane area.
申请公布号 US2015343394(A1) 申请公布日期 2015.12.03
申请号 US201414649679 申请日期 2014.02.13
申请人 TORAY INDUSTRIES, INC. 发明人 HAYASHI Akihiro;OSABE Masahiro;UENO Yoshiyuki
分类号 B01D71/68;B01D69/08;A61M1/34;B01D67/00;A61M1/16;B01D63/02;B01D69/02 主分类号 B01D71/68
代理机构 代理人
主权项 1. A hollow fiber membrane module comprising a built-in hollow fiber membrane including a hydrophobic polymer and a hydrophilic group-containing polymer, the hollow fiber membrane module satisfying the following items: (a) the water content of the hollow fiber membrane is 10% by weight or less relative to the tare weight of the hollow fiber membrane, (b) the hydrophobic polymer contains no nitrogen, the hydrophilic group-containing polymer contains nitrogen, and the nitrogen content of the hollow fiber membrane is 0.05% by weight or more and 0.4% by weight or less, (c) the content of the hydrophilic group-containing polymer in the inner surface of the membrane is 20% by weight or more and 45% by weight or less, and (d) the consumption amount of an aqueous potassium permanganate solution (2.0×10−3 mol/L) used for titrating an eluted substance in 10 mL of a last part of a priming liquid is 0.2 mL or less per 1 m2 of a membrane area.
地址 Chuo-ku, Tokyo JP