发明名称 |
LIGHT WEIGHT PROPPANT WITH IMPROVED STRENGTH AND METHODS OF MAKING SAME |
摘要 |
<p>Methods are described to make strong, tough, and lightweight whisker-reinforced glass-ceramic composites through a self-toughening structure generated by viscous reaction sintering of a complex mixture of oxides. The invention further relates to strong, tough, and lightweight glass-ceramic composites that can be used as proppants and for other uses.</p> |
申请公布号 |
EP2619154(A4) |
申请公布日期 |
2015.11.25 |
申请号 |
EP20110827247 |
申请日期 |
2011.09.15 |
申请人 |
OXANE MATERIALS, INC. |
发明人 |
WU, SHANGHUA;PHAM, JODY;XIE, YUMING;CHATTERJEE, DILIP, K.;MILLER, ANDREW;COKER, CHRISTOPHER, E. |
分类号 |
C04B35/01;C03B19/06;C04B35/10;C04B35/185;C04B35/65;C09K8/80 |