发明名称 |
PREPARATION OF REFINED PIGMENT FROM ELASTOMER |
摘要 |
A pigment and method for making a pigment comprising a milled elastomer, wherein the milled elastomer has a D50 particle size of between about 5 and about 50 microns. A coating of the pigment has a smoothness of about 3 or less. The pigment is prepared by providing an elastomer; and milling the elastomer in the presence of milling media and solvent at a temperature from about 30° C. to about 70° C. The elastomer is insoluble in the solvent. The method for preparing the pigment from an elastomer comprises the steps of: providing an elastomer; and milling the elastomer in a media mill in the presence of milling media and solvent at a temperature from about 30° C. to about 70° C. The diameter of the milling media is from about 0.5 mm to about 10 mm, and the elastomer is insoluble in the solvent. |
申请公布号 |
US2015322247(A1) |
申请公布日期 |
2015.11.12 |
申请号 |
US201514802572 |
申请日期 |
2015.07.17 |
申请人 |
Sun Chemical Corporation |
发明人 |
JOHNSON Steven;NIMMO John;VENTURINI Mike |
分类号 |
C08L9/06;C08F36/06;C08L61/00;C08L7/00;C08L23/16;C08F136/08;C08F36/04 |
主分类号 |
C08L9/06 |
代理机构 |
|
代理人 |
|
主权项 |
1. A pigment comprising a milled elastomer, wherein the milled elastomer has a D50 particle size of between about 5 and about 50 microns and wherein a coating of the pigment has a smoothness of about 3 or less. |