发明名称 銅合金の使用方法
摘要 The invention relates to the use of a copper alloy, composed of (in wt %): 51.8 to 84.0% Cu, 15.5 to 36.0% Zn, 0.35 to 3.0% Sn, 0.12 to 1.5% Fe, 0.02 to 1.0% P, optionally also 0.1 to 2.0% Al, optionally also 0.05 to 0.7% Si, optionally also 0.05 to 2.0% Ni, optionally also respectively 0.1 to 1.0% Mn, Co, optionally also respectively 0.01 to 1.0% As, Sb, and unavoidable contaminants, wherein more than 95% of the structure consist of α-mixed crystal, in which at least iron phosphides and/or iron are embedded as deposition particles, for metallic articles in breeding organisms living in seawater.
申请公布号 JP5808491(B2) 申请公布日期 2015.11.10
申请号 JP20140524283 申请日期 2012.06.15
申请人 发明人
分类号 C22C9/04;A01K63/00;A01K75/00 主分类号 C22C9/04
代理机构 代理人
主权项
地址