发明名称 |
Wrinkle reduction in uncured composite laminates |
摘要 |
Wrinkles are removed from fiber reinforced resin plies of an uncured composite layup by subjecting the wrinkles to vibration and pressure. |
申请公布号 |
US9150700(B2) |
申请公布日期 |
2015.10.06 |
申请号 |
US200812242536 |
申请日期 |
2008.09.30 |
申请人 |
THE BOEING COMPANY |
发明人 |
Guzman Juan C.;McCarville Douglas A.;Rotter Daniel M.;Washburn Todd J.;Willden Kurtis S.;Darrow Donald C. |
分类号 |
C08J5/24;B29C70/30;B29C70/54;B29C35/02 |
主分类号 |
C08J5/24 |
代理机构 |
Yee & Associates, P.C. |
代理人 |
Yee & Associates, P.C. |
主权项 |
1. A method of reducing a wrinkle in a fiber reinforced impregnated resin ply, comprising:
forming a layup comprising said ply, the layup defining a surface; and subjecting the wrinkle to vibrations while applying downward pressure relative to the surface following forming said layup and prior to compacting and curing said layup, said vibrations having a frequency of at least 15,000 Hz and an amplitude of at least 0.0005 inches applied with a flat face head and the vibrations being normal to the surface. |
地址 |
Chicago IL US |