摘要 |
A pressure ranging from 50 Kgf/cm2 to 800 Kgf/cm2 is applied to a pwoder of fine particles of activated carbon, and while the pressure is being applied to the fine particles, pulse voltages are applied between the fine particles for producing electric discharges between the fine particles, and the fine particles are kept at a temperature ranging from 700 DEG C. to 1000 DEG C., thereby sintering the fine particles of activated carbon into an electrode of a porous sintered body. Two such electrodes are impregnated with an electrolyte to produce polarized electrodes, and a separator is sandwiched between the polarized electrodes, thus completing an electric double layer capacitor.
|