发明名称 Low gloss wood for interior trim
摘要 The present disclosure is directed to a light-colored wood component for the interior of an automotive vehicle that includes a UV additive-containing aqueous treating mixture coated onto the wood substrate at a loading ranging between about 84 to about 104 g/m2, and having a low gloss polyurethane-containing topcoat essentially free of UV additives applied to the top surface of the wood substrate. The wood component can have a 60 degree surface gloss rating no greater than about 25 gloss units measured according to ASTM D523-08 test conditions. Methods of producing the vehicle interior component are also disclosed.
申请公布号 US9138777(B2) 申请公布日期 2015.09.22
申请号 US201213662488 申请日期 2012.10.28
申请人 Honda Motor Co., Ltd. 发明人 Alessandro Jessica;McEnhill Corey
分类号 B05D7/08;B05D7/00;B60R13/02;C09D7/12;C09D15/00;C08K5/17 主分类号 B05D7/08
代理机构 Capitol City TechLaw, PLLC 代理人 Capitol City TechLaw, PLLC ;Burkholder Samuel P.;Duell Mark E.
主权项 1. A method of treating a wood substrate comprising: providing a wood substrate having a top surface; contacting a first aqueous treating mixture containing UV additives with the top surface of the wood substrate; and coating the wood substrate with a topcoat composition essentially free of UV additives and comprising a low gloss polyurethane, wherein the first aqueous treating mixture is coated onto the wood substrate at a loading ranging between about 84 to about 104 g/m2, has UV additives present in a concentration of about 2 wt. %, and the topcoat composition comprises a composition which provides a 60 degree surface gloss rating of no greater than about 25 gloss units measured according to ASTM D523-08 test conditions.
地址 Tokyo JP