发明名称 STEEL FOR INDUCTION HARDENING, ROUGHLY SHAPED MATERIAL FOR INDUCTION HARDENING, PRODUCING METHOD THEREOF, AND INDUCTION HARDENING STEEL PART
摘要 A steel for an induction hardening including, by mass %, C: more than 0.75% to 1.20%, Si: 0.002 to 3.00%, Mn: 0.20 to 2.00%, S: 0.002 to 0.100%, Al: more than 0.050% to 3.00%. P: limited to 0.050% or less, N: limited to 0.0200% or less, O: limited to: 0.0030% or less, and the balance composing of iron and unavoidable impurities, wherein an Al content and a N content satisfy, by mass %, Al−(27/14)×N>0.050%.
申请公布号 US2015240335(A1) 申请公布日期 2015.08.27
申请号 US201514707429 申请日期 2015.05.08
申请人 NIPPON STEEL & SUMITOMO METAL CORPORATION 发明人 KUBOTA Manabu;AISO Toshiharu;MIYANISHI Kei
分类号 C22C38/60;C22C38/50;C22C38/48;C22C38/42;C22C38/38;C22C38/34;C22C38/32;C22C38/28;C22C38/24;C22C38/22;C22C38/16;C22C38/14;C22C38/12;C22C38/08;C22C38/06;C22C38/04;C22C38/02;C22C38/00;C21D1/42;C22C38/54 主分类号 C22C38/60
代理机构 代理人
主权项
地址 Tokyo JP