发明名称 ARC WELDING CONTROL METHOD
摘要 As a conventional problem, welding on surface-treated material, such as a zinc-coated steel plate, considerably generates air holes including blowholes and also generates lots of spatters. Present invention provides a method of controlling arc welding performed in a manner that a short-circuit period, in which a short circuit is generated between a welding wire and an object to be welded, and an arc period, in which an arc is generated after release of the short circuit, are repeated alternately. According to the method, welding current is increased from an arc-regeneration-before current to a first welding current at a detection of release of the short circuit such that an increase gradient of the welding current becomes not less than 750A/msec. This suppresses generation of air holes and spatters in welding work on a surface-treated material, such as a zinc-coated steel plate.
申请公布号 EP2905102(A1) 申请公布日期 2015.08.12
申请号 EP20130844324 申请日期 2013.09.30
申请人 PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO., LTD. 发明人 KAWAMOTO, ATSUHIRO;FUJIWARA, JUNJI;HIROTA, YUKINORI;MATSUOKA, NORIYUKI;MATSUI, KAITO
分类号 B23K9/073;B23K9/095;B23K9/12;B23K9/173;B23K9/23 主分类号 B23K9/073
代理机构 代理人
主权项
地址