摘要 |
<p>Provided are a non-flammable FRP panel composition and a construction method using the same. According to the present invention, the composition comprises, with respect to 100 parts by weight of a phenol resin, 50 to 80 parts by weight of composite fiber; 5 to 30 parts by weight of calcium sulfoaluminate; 1 to 10 parts by weight of a lightweight material; 5 to 30 parts by weight of nanoceramic particles; 0.1 to 10 parts by weight of re-emulsifying polymer powder; 0.1 to 10 parts by weight of polyvinyl alcohol powder; 3 to 15 parts by weight of a flame retardant; 3 to 6 parts by weight of a releasing agent; and 2 to 20 parts by weight of a binder. The composition of the present invention prevents a situation that the combustion occurs at the same time when heat and fire occur, thereby preventing a secondary accident, and also being environmental friendly, and having excellent repairing and reinforcing performance.</p> |