摘要 |
PROBLEM TO BE SOLVED: To provide a molded article excellent in moldability as well as impact resistance and heat resistance. ! SOLUTION: There is provided a molded article manufactured by injection molding a polyester resin composition containing 20 to 150 pts.mass of a glass fiber (C) and 1 to 20 pts.mass of a copolymer (D) of α-olefin, an unsaturated glycidyl compound and (meth)acrylic acid ester based on 100 pts.mass of a polybutylene terephthalate resin (A) of 90 to 60 mass% and a polycarbonate resin (B) of 10 to 40 mass%, and the molded article has a bottom surface part recessed by surrounding standing wall with volume of 200 to 20000 cm3 and minimum thickness of 3 mm or less. ! COPYRIGHT: (C)2015,JPO&INPIT |