发明名称 METHOD FOR THE TREATMENT OF STEELWORK SLAG AND HYDRAULIC MINERAL BINDER
摘要 The invention relates to a method for processing steel slag to produce a hydraulic mineral binder with a high hardening potential and to recover iron. There is provision for this purpose to provide a feed product comprising steel slag with MnO. This feed product is further processed as a melt by introducing reducing agent into the melt. A lime saturation factor of between 90 and 110 is hereby to be achieved in the mineral melt portion. Subsequently the melt is cooled in a defined manner and elementary iron is mechanically separated from the solidified melt. The solidified melt is then supplied for use as hydraulic mineral binder. Furthermore the invention relates to a hydraulic mineral binder.
申请公布号 US2015159233(A1) 申请公布日期 2015.06.11
申请号 US201214419167 申请日期 2012.09.06
申请人 Wulfert Holger;Ludwig Horst-Michael 发明人 Wulfert Holger;Ludwig Horst-Michael
分类号 C21C5/36;C04B7/147;C04B5/06;C21B3/08 主分类号 C21C5/36
代理机构 代理人
主权项 1. Method for processing steel slag to produce a hydraulic mineral binder with high hardening potential and to recover iron, comprising the steps: providing a feed product comprising steel slag with iron compounds, in particular in oxide form, and MnO, wherein the MnO may be contained in the steel slag, processing the feed product as melt, incorporating reducing agent into the melt to reduce the iron compounds in order to achieve a lime saturation factor in the mineral melt part of between 90 and 110, wherein the incorporation of the reducing agent is carried out in a non-oxidising atmosphere, defined cooling, wherein the melt solidifies in 15 minutes at the earliest, mechanical separation of elementary iron from the solidified melt, and subsequent supply of the solidified melt with a reduced iron content for use as hydraulic mineral binder.
地址 Berlin DE