发明名称 |
CURRENT COLLECTOR, ELECTRODE STRUCTURE, NONAQUEOUS ELECTROLYTE BATTERY AND ELECTRICAL STORAGE DEVICE, AND METHOD FOR PRODUCING CURRENT COLLECTOR |
摘要 |
A current collector, an electrode structure, a non-aqueous electrolyte battery, and an electrical storage device capable of providing superior shut down function are provided. According to the present invention, a current collector having a resin layer on at least one side of a conductive substrate, wherein: the resin layer has a thermoplastic resin dispersed in a thermosetting resin base material, the thermoplastic resin encapsuling a conductive agent; a value given by (average thickness of the conductive agent)/(average thickness of the thermoplastic resin) is 0.5 to 3; the conductive agent is formulated so that a value of volume % given by (conductive agent)/(conductive agent+thermoplastic resin) is 10 to 50%; and formulation ratio of the thermoplastic resin is 10 to 65%, is provided. |
申请公布号 |
US2015125757(A1) |
申请公布日期 |
2015.05.07 |
申请号 |
US201314397115 |
申请日期 |
2013.05.10 |
申请人 |
UACJ Corporation ;UACJ Foil Corporation |
发明人 |
Kato Osamu;Saito Sohei;Honkawa Yukiou;Wasamoto Mitsuyuki;Kataoka Tsugio;Yamabe Satoshi |
分类号 |
H01M4/66;H01M4/82 |
主分类号 |
H01M4/66 |
代理机构 |
|
代理人 |
|
主权项 |
1. A current collector having a resin layer on at least one side of a conductive substrate, wherein:
the resin layer has a thermoplastic resin dispersed in a thermosetting resin base material, the thermoplastic resin encapsuling a conductive agent; a value given by (average thickness of the conductive agent)/(average thickness of the thermoplastic resin) is 0.5 to 3; the conductive agent is formulated so that a value of volume % given by (the conductive agent)/(the conductive agent+the thermoplastic resin) is 10% to 50%; and formulation ratio of the thermoplastic resin is 10% to 65%. |