发明名称 水硬性固化材の製造方法および耐酸性コンクリートの製造方法
摘要 <p><P>PROBLEM TO BE SOLVED: To provide an acid resistant hydraulic solidifying material for a hardened body reducing equipment cost and raw material cost, to provide a method for producing the same, and to provide acid resistant concrete, iron corrosion-inhibited concrete and reinforcement corrosion-inhibited concrete obtained by using the same. <P>SOLUTION: Caustic soda aqueous solution and silica-containing inorganic powder are blended, so as to be a composition comprising, by weight, a 20 to 40% Na<SB>2</SB>O component, a 30 to 65% SiO<SB>2</SB>component and a 10 to 25% H<SB>2</SB>O component, and in which the molar ratio between the SiO<SB>2</SB>component and the Na<SB>2</SB>O component is controlled to 0.9 to 3.15, and they are mixed, so as to be slurry, and thereafter, the slurry is dewatered or dried, so as to be the raw material for a solidifying material. Further, the raw material for a solidifying material is cured under pressurized steam heated at 130 to 190°C for a prescribed time, and is subsequently pulverized. <P>COPYRIGHT: (C)2009,JPO&INPIT</p>
申请公布号 JP5711556(B2) 申请公布日期 2015.05.07
申请号 JP20110023189 申请日期 2011.02.04
申请人 发明人
分类号 C04B28/26;C01B33/32;C04B14/06;C04B18/14 主分类号 C04B28/26
代理机构 代理人
主权项
地址