发明名称 |
Positive electrode active material, production method thereof and its use |
摘要 |
A method of producing a positive electrode active material, comprising the steps of:
preparing a solution by dissolving, in a solvent, respective predetermined amounts of a lithium source, a M source, a phosphorus source and a X source necessary for forming a positive electrode active material represented by the following general formula (1) having an olivine structure;gelating the obtained solution by addition of a cyclic ether; andcalcinating the generated gel to obtain a carbon-coated lithium-containing composite oxide,wherein the positive electrode active material is represented by the general formula (1):
LixMyP1-zXzO4 (1)
wherein M is at least one element selected from the group consisting of Fe, Ni, Mn, Zr, Sn, Al and Y, X is at least one selected from the group consisting of Si and Al, and 0<x≦2, 0.8≦y≦1.2, 0≦z≦1. |
申请公布号 |
US9017876(B2) |
申请公布日期 |
2015.04.28 |
申请号 |
US201113275858 |
申请日期 |
2011.10.18 |
申请人 |
Sharp Kabushiki Kaisha |
发明人 |
Sueki Toshitsugu;Nishijima Motoaki;Ohira Koji;Esaki Shogo;Tanaka Isao;Koyama Yukinori;Tanaka Katsuhisa;Fujita Koji;Murai Shunsuke |
分类号 |
H01M4/1391;H01M4/58;C01B25/45;H01M4/485;H01M4/505;H01M4/525;C01B31/02;H01M4/131;H01M4/136;H01M4/62;H01M10/052;H01M4/02 |
主分类号 |
H01M4/1391 |
代理机构 |
Nixon & Vanderhye P.C. |
代理人 |
Nixon & Vanderhye P.C. |
主权项 |
1. A method of producing a positive electrode active material, comprising the steps of:
preparing a solution by dissolving, in a solvent, respective predetermined amounts of a lithium source, a M source, a phosphorus source and a X source necessary for forming a positive electrode active material represented by the following general formula (1) and having an olivine structure; increasing a viscosity of the obtained solution by adding a cyclic ether so as to generate a gel; and calcinating the generated gel to obtain a carbon-coated lithium-containing composite oxide, wherein the cyclic ether is used as a carbon source; wherein the positive electrode active material is represented by the general formula (1):
LixMyP1-zXzO4 (1) wherein M is Fe and Zr, X is at least one selected from the group consisting of Si and Al, and 0.8≦x≦1.2, 0.8≦y≦1.2, 0≦z≦0.5. |
地址 |
Osaka JP |