发明名称 SINTERED COMPACT AND INDUCTOR
摘要 PROBLEM TO BE SOLVED: To provide a sintered compact of Z-type hexagonal ferrite, which exhibits L-value or Q-value having low temperature dependence, and to provide an inductor using the same.SOLUTION: A laminate 20 is obtained by using, as starting materials, Z-type hexagonal ferrite, BiOand a glass-based material. The content of BiOis 5-7 pts.wt. to 100 pts.wt. of the Z-type hexagonal ferrite in the starting materials. The laminate 20 is a sintered compact which is obtained by firing the starting materials and contains the z-type hexagonal ferrite as a main phase. The glass-based material is selected from one of silica glass, borosilicate glass, and a mixed material of the two kinds of glass.
申请公布号 JP2015081200(A) 申请公布日期 2015.04.27
申请号 JP20130218313 申请日期 2013.10.21
申请人 MURATA MFG CO LTD 发明人 ODAWARA MITSURU;SHIMIZU YUKIE
分类号 C04B35/26;H01F1/34;H01F17/00;H01F17/04;H01F41/02;H01F41/04 主分类号 C04B35/26