摘要 |
PROBLEM TO BE SOLVED: To provide a method for producing ferrite ceramics.SOLUTION: The method for producing ferrite ceramics includes: preparing a slurry using ferrite powder and flow cast forming the same, followed by calcinating the same to produce ferrite ceramics; a step of de-binder for removing the organic substance in the green compact by heat insulation at 300 to 500°C for 5 hours or more; and a step of calcination for calcinating the green compact finished with the de-binder by heat insulation at 900 to 1000°C for 2 to 5 hours, to obtain a dense ferrite ceramics. |