发明名称 METHOD FOR PRODUCING HIGH SI-CONTENT AUSTENITIC STAINLESS STEEL
摘要 A high-Si content austenitic stainless steel, which exhibits stable acid resistance and excellent corrosion resistance in high-temperature and concentrated nitric acid, has a chemical composition comprising: C: at most 0.04%; Si: 2.5-7.0%; Mn: at most 10%; P at most 0.03%; S: at most 0.03%; N: at most 0.035%; sol. Al: at most 0.03%; Cr: 7-20%; Ni: 10-22%; optionally, one or more types selected from Nb, Ti, Ta and Zr: 0.05-0.7% in total; and the remainder being Fe and impurities, wherein a total amount of B 1 type inclusions measured by a method according to JIS G0555 (2003) Annex 1 "Microscopic Testing for the Non-Metallic Inclusions on the Point Counting Principle" is not more than 0.03% by area%.
申请公布号 EP2738281(A4) 申请公布日期 2015.04.15
申请号 EP20120819675 申请日期 2012.07.26
申请人 NIPPON STEEL & SUMITOMO METAL CORPORATION 发明人 SUKAWA TOMOYUKI;YAMAMOTO SHINNYA;TAKEUCHI KOUICHI;KITA HAYATO;YOSHIDA SHUUJI;TAKETSU KATSUHIKO;SHIBUYA MASAYUKI
分类号 C22C38/58;C22C38/00;C22C38/04;C22C38/06;C22C38/34;C22C38/48 主分类号 C22C38/58
代理机构 代理人
主权项
地址