<p>A yarn includes reinforcing fiber filaments and a resin that is infiltrated into the yarn and can be repeatedly melted and solidified by cooling to room temperature, wherein the filaments of the yarn are at least partially bound to one another by the resin, wherein the yarn contains 2.5 to 25 wt.% of infiltrated resin relative to its total weight, and wherein the infiltrated resin includes a mixture of at least two epoxy resins E1 and E2, E1 having an epoxy value in the range of 2,000 to 2,300 mmol/kg of resin and E2 having an epoxy value in the range of 500 to 650 mmol/kg of resin, and the weight ratio E1:E2 of the epoxy resins E1 and E2 in the mixture is chosen so that the infiltrated resin mixture has an epoxy value between 550 and 2,100 mmol/kg of resin. A preform comprising the yarn, a method for producing the preform and its use in producing a composite are also described.</p> |