发明名称 Selective leach recovery of zinc from a composite sulphide ore deposit, tailings, crushed ore or mine sludge
摘要 Zinc and lead are usually concomitantly present in Zn—Pb ores and tailings. A novel non-polluting hydrometallurgical process for selectively leaching and recovering zinc (Zn) from a composite lead (Pb) and zinc sulphide containing mineral, crushed untreated rock or unconsolidated mineral particles, mill tailings and/or agglomerated or unagglomerated sulphidic zinc containing waste material without necessitating smelting and refining operation has been developed. A combination of selected oxidant and alkali metal hydroxide has been found effective. A leachant consisting of e.g. a mixture of sodium hydroxide (NaOH) and sodium hypochlorite (NaOCl) is employed to selectively dissolve zinc sulphide at high pH at standard temperature and pressure (STP). The kinetics of leaching along with the effect of varying concentration (preferably of sodium hydroxide and sodium hypochlorite) were systematically investigated. Feed ore containing diverse set of minerals e.g. sulphides and carbonates can also be conveniently treated to selectively and almost quantitatively recover zinc as high purity zinc carbonate. This technology can be employed either in-situ or ex-situ based on the amenability of a particular type of mineral deposit or feed ore.
申请公布号 US8961911(B2) 申请公布日期 2015.02.24
申请号 US201113876901 申请日期 2011.09.30
申请人 Yava Technologies Inc. 发明人 Dahal Madhav
分类号 C01G9/00;C22B19/02;C22B3/00 主分类号 C01G9/00
代理机构 Collard & Roe, P.C. 代理人 Collard & Roe, P.C.
主权项 1. A process for selective leaching of zinc from a mixture or ore containing zinc sulfide, comprising: a. contacting the mixture or ore with an aqueous leachant to form a resulting leachate and residual solids from the mixture or ore, said leachant comprising: 1) an oxidant with an oxidation potential to oxidize the sulfur present only to elemental sulfur, and 2) alkali metal hydroxide in an amount sufficient to form soluble alkali metal zincate; b. extending the contact time between leachant and solids to reach a selected zinc recovery and selectivity in the leachate while maintaining operative reagent concentrations; c. separating desired resulting leachate from the residual solids; and d. recovering zinc from the resulting leachate, wherein the oxidant is a water-soluble perchlorate or a water-soluble hypochlorite.
地址 Toronto, Ontario CA