发明名称 SOLAR CELL MODULE SEALING FILM, AND SOLAR CELL MODULE USING SAME
摘要 A solar cell module sealing film including a pair of sealing films which seals a photovoltaic element including a first film disposed on a surface of the photovoltaic element, and a second film disposed on a back surface of the photovoltaic element, in which transmittance of light having a wavelength of 350 nm in the first film is greater than or equal to 80%, and an ultraviolet ray absorber is contained in at least one of the first film and the second film.
申请公布号 US2015047706(A1) 申请公布日期 2015.02.19
申请号 US201214387664 申请日期 2012.03.27
申请人 Miyoshi Masanao;Sugiyama Hitoshi;Kawabe Junya;Hirano Tatsuya 发明人 Miyoshi Masanao;Sugiyama Hitoshi;Kawabe Junya;Hirano Tatsuya
分类号 H01L31/048 主分类号 H01L31/048
代理机构 代理人
主权项 1. A solar cell module sealing film, comprising: a pair of sealing films which seals a photovoltaic element including a first film disposed on a surface of the photovoltaic element, and a second film disposed on a back surface of the photovoltaic element, wherein transmittance of light having a wavelength of 350 nm in the first film is greater than or equal to 80%, an ultraviolet ray absorber is contained in at least one of the first film and the second film, and a transmittance attenuation rate of the first film at the time of performing a test by the following testing methods (1) to (5) is less than or equal to 10%, <Testing Methods> (1) obtaining a test plate by making the first film having a thickness of 0.5 mm, a length of 50 mm, and a width of 50 mm, and the second film having a thickness of 0.5 mm, a length of 50 mm, and a width of 50 mm be in contact with each other in a width direction, and by sandwiching the first film and the second film by two glass plates having a thickness of 0.5 mm, a length of 50 mm, and a width of 50 mm, (2) measuring the transmittance of the light having the wavelength of 350 nm in a portion of 5 mm in a direction of the first film from a seam between the first film and the second film in the test plate (a portion having a measurement area in the shape of a quadrangle of 10 mm in width×5 mm in length), (3) heating the test plate at 85° C. for 14 days, (4) measuring the transmittance in the test plate by using the same method as (2), and (5) setting the transmittance in (4) at the time of setting the transmittance in (2) to 100 to the transmittance attenuation rate.
地址 Kitaadachi-gun JP