发明名称 |
LOW ALLOY STEEL |
摘要 |
A low alloy steel, containing, by mass percent, C: 0.01 to 0.15%, Si: 3% or less, Mn: 3% or less, B: 0.005 to 0.050%, and Al: 0.08% or less, and the balance being Fe and impurities, wherein in the impurities, N: 0.01% or less, P: 0.05% or less, S: 0.03% or less, and O: 0.03% or less. In the alloy steel, a HAZ has excellent resistance to embrittlement attributable to hydrogen such as stress corrosion cracking in wet hydrogen sulfide environments. |
申请公布号 |
US2014348695(A1) |
申请公布日期 |
2014.11.27 |
申请号 |
US201214370999 |
申请日期 |
2012.12.17 |
申请人 |
NIPPON STEEL & SUMITOMO METAL CORPORATION |
发明人 |
Hirata Hiroyuki;Kobayashi Kenji;Omura Tomohiko;Kawano Kaori;Tomatsu Kota;Ogawa Kazuhiro |
分类号 |
C22C38/58;C22C38/48;C22C38/46;C22C38/44;C22C38/42;C22C38/38;C22C38/32;C22C38/24;C22C38/14;C22C38/12;C22C38/08;C22C38/06;C22C38/04;C22C38/02;C22C38/00;E21B17/00;E21B17/01;C22C38/54 |
主分类号 |
C22C38/58 |
代理机构 |
|
代理人 |
|
主权项 |
1. A low alloy steel, containing, by mass percent,
C: 0.01 to 0.15%, Si: 3% or less, Mn: 3% or less, B: 0.005 to 0.050%, and Al: 0.08% or less, and the balance being Fe and impurities, wherein in the impurities, N: 0.01% or less, P: 0.05% or less, S: 0.03% or less, and O: 0.03% or less. |
地址 |
Tokyo JP |