摘要 |
PROBLEM TO BE SOLVED: To provide a polyacetal resin composition having excellent impact resistance and sufficiently suppressing the generation of a formaldehyde, and a molding obtained by using the same. SOLUTION: The polyacetal resin composition is obtained by combining 1-120 pts.mass of thermoplastic polyurethane (B) and 0.01-5 pts.mass of a formaldehyde capturing agent (C) that has formaldehyde reaction nitrogen to 100 pts.mass of polyacetal resin (A), wherein the thermoplastic polyurethane contains 0.10 mass% or less of a remaining isocyanate amount, has a water content of 3,000 mass ppm or less, and shows a melt viscosity of 200,000 poise or more at 180°C. COPYRIGHT: (C)2013,JPO&INPIT |