发明名称 Windmill propeller blade and method of making same
摘要 A windmill blade which comprises reinforcing fibers in a toughened resin matrix. The resin matrix is made from a composition which comprises (a) one or more epoxy resins and/or one or more epoxy vinyl ester resins, (b) one or more reactive diluents, and (c) at least one amphiphilic block copolymer. The amphiphilic block copolymer comprises at least two different polyether blocks and is present in the composition in an amount of from about 0.5% to about 10% by volume, based on the total volume of the matrix composition.
申请公布号 US8829101(B2) 申请公布日期 2014.09.09
申请号 US200912937304 申请日期 2009.05.04
申请人 Dow Global Technologies LLC 发明人 Jacob George;Pham Ha Q.;Dettloff Marvin L.;Hunter Gary A.;Turakhia Rajesh
分类号 C08J5/04;F03D1/06;C08L63/10;C08L63/00;C08L71/02 主分类号 C08J5/04
代理机构 代理人
主权项 1. A windmill blade which comprises reinforcing fibers in a resin matrix, wherein the matrix is made from a matrix composition which comprises (a) one or more epoxy resins, (b) one or more reactive diluents, and (c) at least one amphiphilic block copolymer which comprises at least two different polyether blocks and is present in the composition in an amount of from about 0.5% to about 10% by volume, based on a total volume of the matrix composition; wherein the amphiphilic block copolymer, component (c), comprises at least one polyether block A and at least one polyether block B; wherein the polyether block A is independently selected from a polybutylene oxide block, a polyhexylene oxide block, a polydodecylene oxide block, and a polyhexadecylene oxide block; and wherein the polyether block B is independently selected from a polyethylene oxide block, a polypropylene oxide block, and a poly(ethylene oxide-co-propylene oxide) block; wherein a weight ratio of the polyether block A to the polyether block B in the amphiphilic block copolymer, component (c), is from about 10:1 to about 1:10; wherein the epoxy resin, component (a), is present in an amount of from about 30% to about 95% by volume, based on the total volume of the matrix composition; wherein the reactive diluent, component (b), is present in an amount of from about 5% to about 25% by volume, based on the total volume of the matrix composition; and wherein the amphiphilic block copolymer, component (c), is present an amount of from about 1% by volume to about 5% by volume, based on the total volume of the matrix composition.
地址 Midland MI US