发明名称 |
Method for manufacturing lithium ion secondary battery, and packaging thereof containing pre-charged lithium ion secondary battery |
摘要 |
There is provided a lithium ion secondary battery exhibiting a high capacity retention rate over a long period. There is also provided a method for manufacturing a lithium ion secondary battery including a positive electrode, a negative electrode containing a negative electrode active material layer containing a graphite, an aprotic electrolyte solution containing a sulfonate ester having at least two sulfonyl groups, and a packaging material including a laminate film involving the positive electrode, the negative electrode and the aprotic electrolyte solution, the method including: enclosing the positive electrode, the negative electrode and the aprotic electrolyte solution in the packaging material to fabricate a lithium ion secondary battery before pre-charge; pre-charging the lithium ion secondary battery; and opening the enclosure of the packaging material of the lithium ion secondary battery after pre-charge, thereafter vacuum sealing the packaging material, and regularly charging the lithium ion secondary battery after pre-charge, wherein the current for the pre-charge is 0.05 to 0.25 C, and the voltage thereof is 3.3 to 3.5 V. |
申请公布号 |
US8814955(B2) |
申请公布日期 |
2014.08.26 |
申请号 |
US201013510819 |
申请日期 |
2010.09.30 |
申请人 |
NEC Energy Devices, Ltd. |
发明人 |
Kumeuchi Tomokazu;Zama Koichi;Kono Daisuke |
分类号 |
H01M10/44 |
主分类号 |
H01M10/44 |
代理机构 |
Sughrue Mion, PLLC |
代理人 |
Sughrue Mion, PLLC |
主权项 |
1. A method for manufacturing a lithium ion secondary battery,
the lithium ion secondary battery comprising: a positive electrode; a negative electrode comprising a negative electrode active material layer comprising a graphite; an aprotic electrolyte solution comprising a sulfonate ester having at least two sulfonyl groups; and a packaging material comprising a laminate film involving the positive electrode, the negative electrode and the aprotic electrolyte solution, and the method comprising: enclosing the positive electrode, the negative electrode and the aprotic electrolyte solution in the packaging material to fabricate a lithium ion secondary battery before pre-charge; pre-charging the lithium ion secondary battery at a current value of between 0.05 C and 0.25 C to a voltage between 3.3 V and 3.5 V; and opening the enclosure of the packaging material of the lithium ion secondary battery after pre-charge, thereafter vacuum sealing the packaging material, and regularly charging the lithium ion secondary battery after pre-charge. |
地址 |
Kanagawa JP |