发明名称 |
METHOD FOR DETERMINATION OF BRITTLE CRACK PROPAGATION STOPPING PERFORMANCE IN HIGH-INTENSITY THICK STEEL PLATE |
摘要 |
<p>A method of determining brittle crack propagation arrestability of a high-strength steel plate includes the steps of: performing a large-scale test and a composite small-scale test using standard steel; calculating a correlation model of the result of the large-scale test and the result of the composite small-scale test using the standard steel; performing the composite small-scale test using a steel specimen; and estimating the brittle crack propagation arrestability of the steel specimen by substituting the result of the composite small-scale test using the steel specimen into the correlation model. The composite small-scale test includes the sub steps of: (a) sampling a surface-small-scale-test-piece including a surface part of a steel plate; (b) sampling inner-small-scale-test-pieces from one or more inner regions not including the surface part of the steel plate; (c) performing a drop weight test using the surface-small-scale-test-piece; and (d) performing a small-scale test of measuring a brittle fracture percentage or absorbed energy using the inner-small-scale-test-pieces. The composite small-scale test includes performing the small-scale test on the surface-small-scale-test-piece and the inner-small-scale-test-pieces through the use of different methods.</p> |
申请公布号 |
EP2508866(A4) |
申请公布日期 |
2014.05.14 |
申请号 |
EP20100847032 |
申请日期 |
2010.09.03 |
申请人 |
NIPPON STEEL & SUMITOMO METAL CORPORATION |
发明人 |
ISHIKAWA TADASHI;INOUE TAKEHIRO;NAKASHIMA KIYOTAKA;SHIRAHATA HIROYUKI;OOTANI JUN;ITOH AKIRA |
分类号 |
G01N3/30;C21D8/02;C22C38/00;C22C38/06;C22C38/60 |
主分类号 |
G01N3/30 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|